鞋类生产缺陷中英文对照

更新时间:2023-05-19 05:58:26 阅读: 评论:0

鞋类产品缺陷中英文对照
Abrasion磨损
 
Angle on insole中底发角
 
back height 后跟高度
 
Back strap too high(low,long,short)后拉带太高
 
bottom dirty大底不洁
 
Broken thread断线
 
Cement on heel鞋眼沾胶
 
Cementing comes off脱胶
 
Cementing no good接着力不佳
 
chip碎屑
 
Cleanness not enough清洁度不佳
 
Color not matching色差
 
Color variation色差
 
Crooked back stay 后套歪斜
 
Crooked upper鞋面弯曲
 
Crooked屈曲,不平顺商务英语学习网站
 
Damaged upper鞋面破损
四级准考证号忘了怎么办 
dirty 脏的
 
father的音标Flatten变平
 
gaping 缝隙
 
get mildew发霉
 
Gore too weak松紧带弹性不佳
 
hairy 起毛
brush的复数形式 
Heel not straight后套不正
 
开发英语>预期结果Lasting off center攀歪
 
Loo thread脱线
 
Not in pair不配双
 
Outsole not smooth大底不平
 
over cemented溢胶
 
Pinch in 缩进去
 
Rough粗糙
 
Shank not straight铁心不正
 
Shank too loo铁心太松
 
smeary污染
 
sole adhesion大底欠胶
top of the world 
Sole come off底脱胶
 
Sole laying not proper(centered)贴底不正确
 
Stitching not even车不平均
 
Stitching not on the mark不照记号齿车
 
Toe broken down鞋头凹陷
 
Tricot shows up特丽可得露出来四级查询时间
Turn yellow变黄 
Turn dark变黑 
首尔艺术高中Vamp length鞋头大小 
Vamp open up鞋面掀开 
Vamp split off 鞋面爆开 
Vamp wrinking鞋面皱纹 
Wrapping not even攀帮不均匀 
Wrapping not tight攀帮不紧 
Wrong colour颜色错误 
Wrong cutting裁断错误 
Wrong last 楦头错误 
PPER DEFECT CATEGORY - U  COUNTER DEFECTS - CO   
後套瑕疵 
1. Counter sheet not lasted under insole.港寶片未拉到中底上 
2. Wrinkled counter caud either by poor lasting or by wrinkled chemical sheet. 
拉幫不良或港寶片皺造成起皺。 
3. Soft chemical sheet due to wrong material or wrong primer.   
港寶片品質不良或處理不良導致港寶片發軟。
4. Crooked chemical sheet.港寶片位置歪斜 
儿童动画故事5. Low positioned chemical sheet.港寶片位置太低
6. Blisters on counter.後套有氣泡 
7. Back height not uniform within pair by 2.0-mm or more.後套高度不一致達2mm或更多
8.Other counter defects.其它後套瑕疵

本文发布于:2023-05-19 05:58:26,感谢您对本站的认可!

本文链接:https://www.wtabcd.cn/fanwen/fan/90/114185.html

版权声明:本站内容均来自互联网,仅供演示用,请勿用于商业和其他非法用途。如果侵犯了您的权益请与我们联系,我们将在24小时内删除。

标签:鞋面   寶片   错误   處理   鞋类   网站   预期   故事
相关文章
留言与评论(共有 0 条评论)
   
验证码:
Copyright ©2019-2022 Comsenz Inc.Powered by © 专利检索| 网站地图