锂离子电池技术英文词句
2.3 asmbly line process(5/15)流水线工艺
film loading-vacuum on-film folding-sliding jig backward-top cutting-sliding jig forward-
vacuum off-film unloading
放上包装膜—抽真空—包装膜折叠-分切夹心的后端-剪掉顶部-分切夹心的前段-释放真空-拿下包装膜station 岗位two station 两个岗位
folding 折叠guide type 指导方式
top cutting 顶部剪切knife 刀片
2.3 asmbly line process(6/15)流水线工艺
j/r loading-vacuum on-j/r jig backward-bottom former up-upper former down-
放极组-抽真空-极组夹具放在后端-模板末端在上面-顶端在下面-
heating forming-former up,down-j/r jig forward-vacuum off-j/r unloading
加热模板-模板上下翻转-极组夹具朝前-释放真空-取下极组
station two station
岗位两个岗位
heating forming pressing time,pret timer
加热模板施压时间施压次数
global warmingtemperature thermocouple
温度热电耦
time:mmin,2~max.3c
时间:
press force :40~50kg
压力
temperature:150℃
温度
2.3 asmbly line process(7/15)流水线工艺中南大学四六级报名
film loading-fim clamp-sliding jig backward-edge pushing-tab clamp-tab unclamp-
放上包装膜-包装夹具-分切极组末端-整边-放极耳夹具-卸下极耳夹具
sliding jig forward-cell unloading
分切极耳前端
station two station
heat aling top
热封
aling thickness control(micrometer)
热封厚度控制(毫米)
aling control pressing time,pret timer
热封控制施压时间施压次数
precision regulator
精度校准
temperature, thermocouple
温度热电耦
time :min.2~max.3c时间
press force:250kg
压力
temperature:180~250℃
温度
2.3 asmbly line process(9/15)流水线工艺
cell loading-vacuum on-sliding jig backward-side cutting-feeding-tab cutting-
放上电芯-抽真空-滑动夹心后端-裁边-流入下工序-剪极耳
sliding jig forward-cacuum off-cell unloaing
滑动夹心前端-释放真空-取下电芯
station two station
side cutting knife
side cutting force 100kg
tab cutting knife
tab cutting force 100kg
2.3 asmbly line process(10/15)流水线工艺
cell loading-sliding jig backward-vacuum pad down-open-needle down-e/l filling(e/l-needle up-needle up-vacuum pad up-sliding jig forward-cell unloading
station two station
e/l supply 3kuter sub-tank on equipment
metering pump hi -bar pump,hbd-2bc-17
accuracy; under 3.0;±0.1g
ocer 3.0; ±3.5g
2.3 asmbly line process(11/15)流水线工艺
cell loading-sliding jig backward-jig backward-jig up-vacuum(vacuum chamber)-
放上电芯-滑动夹心后端-夹心向后-再向上-抽真空-
gelangaling block forward-aling
过来人网热封前端- 密封
--aling block backward-jig down-silding jig forward-cell loading-formation
热封后端- 夹心翻转向下-滑动夹心前端-取下电芯-成型
station two station
vacuum source 740mmhg max.vacuum pump
aling control pressing time pret tiomer
pressing force, precision regulator
temperature, thermocouple热电偶
time:min.3~max4c
press force:250kg
temperatrure:180~250℃
2.3 asmbly line process(12/15)流水线工艺
cell loading-conveyor drive-numbering-numbering-head down-vacuum on-
放上电芯- 启动传送带- 编号码-编号码-电芯朝下-抽真空
head up-head forwward-head down-vacuum purge-head up-cell unloading
电芯朝上- 电芯朝前- 电芯朝下-真空净化- 电芯朝上-取下电芯
speed controller motor 25W
英语四六级报名入口官网numbering ink jet printer
cell unloading magacine
2.3 asmbly line process(13/15)流水线工艺
piercing-cell loading-sliding jig backward-jig up-vacuum°assing-
穿透??- 放电芯-滑动夹心后端-夹心向上- 抽真空&脱气
aling block forward-aling-aling block backward-jig down-sliding jig forward-cell loading
热封前端- 热封–热封后端-滑动夹心前端–取电芯
station two station
piercing ∮6hole
vacuum source 750mmhg max.vacuum pump
aling comtrol pressing time ,pret timer
pressing force,preision regulator调整压力
temperature,thermocouple(温度热电偶)
time: min.3~max.4c时间
press force:250kg(压力)
temperature:180~250℃(温度)
2.3 asmbly line process(14/15)流水线工艺
cell loading-vacuum on-sliding jig backward-cutter down-cutting-cutter up-
放电芯-抽真空-滑动夹心后端-切割刀具向下-切割-切割刀具向上
sliding jig forward-vacuum off-cell loading
滑动夹心前端- 释放真空-取下电芯
laycan电池封口--
cutting(切断) knife(刀)
2.3 asmbly line process(15/15)流水线工艺
cell loading-ist folding-2nd folding-heat pressing-3nd folding-4th folding(sicing)
放电芯- 第一次折叠-第二次折叠-热压-第三次折叠-第四次折叠
cell unloading
取下电芯
manual-loading-2st foliding-heat pressing-3nd folding-4th folding
手工–放上- 第二次折叠- 热压- 第三次折叠- 第四次折叠
scat
cell transfer linear transfer
folding actuator pneumatic actuator
heat pressing pressing time,pret timer
pressing force
precision regulator
temperature, thermocouple
time:min.2~max.3 c
press force:40kg
temperatrure:80~100℃
2.3 asmbly line process(1/6)流水线工艺
jelly roll supply-jelly roll loading-cell alignment-tab straightening-
提供极组-放上极组-电芯排列好-将极耳伸直
alant aling(alant film supply)-alant aling(alant film supply)-final aling- 密封胶密封(密封膜供给)-密封胶密封(密封膜供给)-最终的密封
alant film check-tab forming-jelly roll unloading(ng unloading)
检验密封膜-极耳成型-取下极组
2.3 asmbly line process(2/6)流水线工艺
al-foil supply-pre heating(contact)-pouch forming---pouch punch out-
—供应箔(铝塑膜)-预热(连接)-成型成袋状- 袋状膜冲压打孔
pouch loading(pouch pin hole check)-pouch loading-ist folding-lst folding-2nd folding-
放上袋状膜(检验针孔)-放上袋状膜- 第一次折叠-第二次折叠
top cutting(ng unloading)-jelly roll inrtion(jelly roll alignment-jelly roll loading)—
剪掉顶部—插入极组(调整极组-放上极组)
3nd folding-pre heat aling-package unloading
第三次折叠-预热密封—取下包好的电芯
2.3 asmbly line process(3/6)流水线工艺
cell loading-lst top aling--2nd top aling-top cooling-side aling-side cooling-
放上电芯-第一次顶部密封-第二次顶部密封-顶部冷却—封边—两边冷却
side cutting-short check-cell unloading-ng unloading
裁边- 测短路—取下电芯—ng是什么啊
package loading-pre weighing-package opening-e/l filling(e/l dispensing e/l supply tank) 放上包装好的电芯—预称重—打开电芯--- 注液(分配电解液电解液供给罐)
--lst vacuum-2nd vacuum --lst aling-2nd aling-plst-weighing-package unloading-
第一次抽真空---第二次真空---第一次密封---第二次密封------称重---取下电芯package loading-package aging--formation
放上电芯---电芯老化-----化成
cell loader-cell-loading-piercing-vacuum°assing heat aling-2nd aling-
装电芯设备-电芯-装上电芯—穿透(??)-抽真空& 脱气热封—第二次密封
side trimming-cell unloading
修边--- 取下电芯
cell loading-lst folding-2nd folding-3rd folding-4th folding-5th folding(sizing)-
放电芯---第一次折叠---第二次折叠---第三次折叠---第四次折叠---第五次折叠(量尺寸)5th folding(sizing)-tab cutting-height&vision check-final weighging-final weighting-
第五次折叠(量尺寸)---剪极耳---检验高度&视觉---最后称重
ng rejection-cell unloading-cell unloading-cell palleticing
挑选,排除---取下电芯--- (用托盘)搬运电芯
1.1 asmbly line specification –products流水线特殊产品
can type(壳体类型) aluminum can(A3003) 铝壳(材质A3003)
conventional prismatic type ,not oval type 传统的方型,不是椭圆型model of cell电池型号basic design model:xx-yy—zz基本设计型号:XX-YY-ZZ range 范围w:30~34mm t:4.0 ~10mm h:40~67mm宽:厚:高:cathode tab正极耳AL,t0.08~0.12mm,w3/4mm铝带,厚度0.08~0.12mm宽度3/4mm welding to top cap with ultrasonic welder 用超声波焊接机超焊在极片头部
anode tab负极耳ni,t0.08~0.12mm,w3/4mm镍带,厚度0.08~0.12mm宽度3/4mm welding to top cap with resistance spot welder用阻抗点焊机焊在极片头部
can am welding壳盖的缝隙焊接side welding侧面焊接
top insulator 顶部绝缘片injection molded注液模具
bottom tape wrapping底部贴胶纸pp-tape,same as j/r wrapping tape, roll,w:28~32mm
t:0.05~0.10mm o.d:200mm core id:3inches
for xx30zz width 28mm,for xx34zz width 32mm
fill port welding 补焊砂眼AL Ball (Al050,∮1.37±0.03mm),lar am welding 激光焊接
e/l filling accuracy 精确注液量under 3.0g; ±0.1g
over 3.0g ±3.5g r/l filling volume:1~7g 注液量范围1~7g
model change exchange tool,jig, carrier&tray搬运工具,夹具,搬运盒&托盘
option:only carrier&tray (others:sutomatically adiusted其它:适当调整)
tray托盘jr极组(256pcs),can壳(300pcs),cap盖帽(100pcs),(rivet)
all trays are prepared ur
1.2 asmbly line specification –equipment流水线特殊设备
line tact time 流水线标准工时 2.0(30ppm)
Drive mechanism 发动装置cam,ac rvo drive&air actuator
electrical power 电源286kva,3p-380v±10%,50hz±1hz
pneumatic source 气源13300l/min,0.6mpa (include welding jig cooling包括焊接模具冷却)
nitrogen gas 氮气285 l/min, 0.6mpa(for lar welding shield gas激光焊接防护气)
模糊数学模型lar cooling water激光焊冷却水320 l/min,below25℃
fume collector 烟、气收集罐400cfm,explosion-proof type for al-fume,outdoor type
broken是什么意思fume suction main piping 抽气主管道系统 4 inch
exhaust piping排气管道系统5inch
dry air piping干燥气管道系统5inch
dry chamber(total) 干燥室20.78m3
total weight总重量14.8ton(approx大概),(not include lar welder不包括激光焊接机)
floor load 场地负荷1500kg/m2
功夫熊猫原型是姑娘dry room height干燥室高度2500mm(min)
can am welding壳盖的缝隙焊接side welding侧面焊接,welding speed 焊接速率10~15mm/c.(approx) cartesian robot stage
electrolyte filling process注电解液工序40station-80 jig index unit,vacuum真空&pressurize加压
elctrolyte filling range注液范围depend on internal dead space of cell design根据电池设计内部的绝对空间
hbd-2bc ries of hibar pum, japan hibar
leak check 测漏differential pressure check system,100pa max.不同压力测试系统,最大为100pa accuracy:+/-0.5%精确度
need test actual work 需要通过实际操作测量
2.1 asmbly parts name&composition
ball-top cap asmbly盖板流水线(t/c)--top insulator顶部绝缘片(t/l)-cathode正极耳(al-tab铝带)-anode负极耳(ni-tab镍带)-
bottom tape底部胶纸(b/t)-jelly roll极芯(j/r)-aluminum can铝壳
2.2 asmbly process basic specification装配过程概述
3.1 prismatic lib asmbly process
bottom tape底部胶纸-jelly roll inrtion极芯入壳-top insulator顶部绝缘片-tab forming极耳修整-top-cap welding顶部极耳焊接-
top cap folding极耳折叠-top cap tting卡极耳-am welding焊缝焊接-leak check测漏-electrolyte filling注液-
ball inrtion压钢珠-fill port welding补焊砂眼()
3.2 asmbly line process(1/8)
can supply供应壳non dust paper tray无尘的纸盘
can tray size装壳的盘子尺寸270*212*22/32h
tray capacity盘子容量423048-450can/tray