8.你提供的3D产品图有的地方没有出模角,有的地方胶位太厚,有的地方胶位太溥,这些产品问题我们可以自己修改吗?修改后会给交给你确认。
There is no draft angle in the 3D model some areas are too thick and some are too thin.
标志位Can we modify them by ourlves? We will nd you the updated drawing for approval.
9.按你们提供的缩水率千分之五,这个模具的尺寸已经做到了模具图面要求。但注塑出来的产品不符合你们的产品图。请确认你们的材料的缩水率是否正确?
According to the shrinkage rate .005” the mold has been done in the right dimension but the part falls short to your part print(the actual dimensions are out of tolerances) are you sure the shrinkage is right?
10.产品的这个位置太小,导致模具钢料太溥,能够加宽这个位置吗?
This position is too small and will cau thin steel can we widen it here?
11.斜顶与后面的柱位空间太小,斜顶在运动时会干涉到柱子,能移动这个柱子的位置吗?
The space(room) is too small between the lifter and the boss. The angular lifter interferes with the boss during ejection(when moving). Plea consider changing the position of the
boss.
12.这个筋骨位胶厚太溥,而且高度偏高,注塑时很难填充这个筋位,可以增加这个筋骨位的厚度吗?
The rib here is too thin and relatively high so it will be difficult to fill(走胶) here during the injection process can we increa the thickness of this rib?
13.你是想将此筋骨位的高度加高/减低吗?加胶的位置我们将用铜公放电加深。但减胶的位置有两种做法,1、做镶件;2、烧焊;因为镶件的底部有运水,我们简单的做法是烧焊处理,你可以接受吗?
Are you going to increa or decrea the plastic(material) on this rib?
For increasing plastic we will u EDM.
For decreasing plastic there will be two options. One is to make inrts; the other is to weld the tool.
Becau there is water line under the inrt is that OK?
14.这个样板的筋骨位底部烧焦,是因为排气不良,我们可以在筋骨位的中间增加一个镶件。
The bottom of the rib was burned due to poor venting we can add an inrt in the middle of the rib to improve it.
15.重做镶件大约需要5-6天时间,你能接受吗?
It will take about 5 or 6 days to re-do the inrt is that OK?
16.产品的这个面我们已经做了晒纹处理,如果需要加胶,这个面我们需要重新外发晒纹。可能需要几天的时间。
所以我们直接以铜公放电的火花纹取代你要求的纹路,你可以接受吗?
We have already textured this side. If we add material it will take a few days to remake the texture. So we suggest using the EDM( spark) finish instead of texturing is that OK?
17.模具是用公制/英制的配件?需要备用件吗?
Are the mold parts in inches or mm? Do they need spare parts?
18.模具上铭牌上的刻字内容是由你们提供吗?你们什么时候可以这些刻字资料。
Will you provide the engraving content of the mold label? Plea advi it asap.
19.可否提供此模具生产时,注塑机的型号及相关资料。如:啤机大小、呵林柱尺寸、顶棍孔尺寸等传达室
Can you provide the specifications of your injection machine? Such as the press size tie bar space Konck-out(K.O.)/ejector rods holes pattern.
byaccident20.这个问题我需要同其它同事商议会再答复你。
I will discuss it with my colleagues and reply asap.
21.我们将尽力达成你的计划,如有异常,会及时通知你。
We will try our best to meet/ reach your plan. For any problems we will notify you immediately/promptly.
22.这个产品的长度为330.12MM宽度为78.96MM高度为45MM.胶厚为2MM重量为70.63g试模注塑机型号为250吨胶料颜色为黑色产品外表面晒纹处理内表面为抛光.需要日期章、环保章、材料章.前后模用2344氮硬,斜顶和行位座用738H,以上模具信息正确吗?请确认!
Plea check the information below and comment/approve.
L. W. H =330.12 x 78.96 x 45MM
Thickness - 2MM.
talonWeight - 70.63g
Press size - 250T
Color of the T1 samples - black.
现在Outer/visible surface finish – texture; inner side – polishing.
Date code recycle stamp and material I.D. needed.
CAV & Core - 2344 nitrided steel; Lifter and slider shelf/baxxxx/retainer - 738H.
23.现在到了吃午钣的时间,我们下午再继续好吗?
Lunch time shall we go for lunch now? We can discuss the project later.
日语同声传译
24.和滑块干涉的倒勾请加料填平至滑块可以顺利滑动
The undercut area interferes with the slide block so we suggest adding material to help the slider move smoothly.
25. 加胶太多 (The added wall/thickness is too much)
26. 加肉面积太大 (The added area is too wide.)